Hoffman Amplifiers Tube Amplifier Forum

Amp Stuff => AmpTools/Tech Tips => Topic started by: tubesornothing on June 23, 2009, 07:53:49 pm

Title: MG Chemicals "no clean" solder
Post by: tubesornothing on June 23, 2009, 07:53:49 pm
Currently I use a kester 44 leaded 60/40 rosin core solder.  I dont want to clean up the rosin any more, and I see that there are "no clean" solders.  Anyone try any? Is it really no clean?
Title: Re: MG Chemicals "no clean" solder
Post by: PRR on June 25, 2009, 12:39:20 am
> I dont want to clean up the rosin any more

So don't.

Unless you are building a rocket-submarine, Kester flux will not cause a problem.
Title: Re: MG Chemicals "no clean" solder
Post by: samwheat on June 28, 2009, 09:10:49 am
I use this ...... http://www.alliedelec.com/Search/ProductDetail.aspx?SKU=8330029&MPN=24-7068-7606